Tumbling

How to Use a Rock Tumbler: Grit Stages

Rock tumbling step by step: choosing rocks of similar hardness, coarse to polish grit stages, cleaning between stages and timing.

Quick answer

Rotary rock tumbling usually runs in four stages: coarse grit to shape, medium and fine grit to smooth, and polish to shine, each lasting about a week. Tumble rocks of similar hardness together, fill the barrel about two thirds, and clean rocks and barrel thoroughly between stages. Never pour grit slurry down a drain, as it can clog plumbing.

Patience and cleanliness make the difference between dull and glassy stones.

The four stages

Stage Grit Purpose Typical time
1 Coarse (60/90) Shape and round 1 week or more
2 Medium (120/220) Smooth 1 week
3 Fine (500 to 1000) Pre-polish 1 week
4 Polish Shine 1 week

Tips

  1. Group rocks by hardness.
  2. Fill the barrel about two thirds full.
  3. Add water just below the top of the rocks.
  4. Clean everything between stages; leftover coarse grit scratches polished stones.
  5. Dispose of slurry in the trash, not the drain.

Rotary vs vibratory

  • Rotary: shapes rough rocks, slower, cheaper.
  • Vibratory: faster, keeps shape, better for polishing pre-shaped stones.

Wear eye protection when handling rough rocks.

Common questions

How long does rock tumbling take?

In a rotary tumbler, often around four weeks or more in total. Vibratory tumblers are faster but do less shaping.

Which rocks tumble best?

Agate, jasper and other quartz-family rocks at Mohs 7 tumble well together.